Mike Casselton
Forming 220 Russian to 6 ppc
Wednesday, October 30, 2019, 11:38

Scotty,
Prime them,
Get some powder somewhere between AA-1680 and H-335.
Fill it up to the neck and top off with a hunk of cotton ball.
Fire them and voila, you got a 6 PPC.

You can also fire them as 220 russian with cheap bullets and they will form about 98%.

Once fireformed, they are easy to work with.

Also, for more info on forming, check out the cartridges section on accurate shooter.com

Lastly,
If you get desperate, I have some actual Norma and Sako 6PPC cases available.