while the flame is going. Your mixture sounds like it is bulky and clogging up the sprue hole.
-
mould problem
- carl hackney, 2021-01-18, 10:00
- thanks guys - carl hackney, 2021-01-19, 06:54
-
Carl, if you have tried everything listed
- Mark Conner, 2021-01-18, 13:58
- FWIW LEE sprue plate screw is left hand thread. - WB, 2021-01-18, 20:45
- try fluxing it again and really stirring it - Gary Reeder, 2021-01-18, 11:33
- In the winter, i heat the sprue cutter - steve todd, 2021-01-18, 10:39
-
That sounds like a too cold pour.
- WB, 2021-01-18, 10:07
-
i tried more tin and hotter temps but made little to no
- carl hackney, 2021-01-18, 10:27
-
I’m still inclined toward cool alloy or sprue plate.
- WB, 2021-01-18, 11:15
- Might of gotten some zinc in the mix (nm) - Jk, 2021-01-19, 12:28
-
I’m still inclined toward cool alloy or sprue plate.
- WB, 2021-01-18, 11:15
- Also on LEE moulds, they need lubrication. - WB, 2021-01-18, 10:10
-
i tried more tin and hotter temps but made little to no
- carl hackney, 2021-01-18, 10:27