Jim Taylor
I drop 'em on a folded-up towel ..
Wednesday, March 02, 2022, 06:36

I have done water quenching and I also did heat-treating when I was running the 454 pretty hot. But it's not needed with a decent alloy when shooting at standard velocities in the guns I am using now.