WB
You mentionte that, heat with a propane torch first?
Saturday, February 20, 2021, 18:23

Then pour? I got some success with pure lead noses by doing that but it was a real trick. I worked a deal with Carl and bought that .375 mold that I have the special nose piece mould for. He was kind enough to sell to me and re-unite the set.

I think his is a 265 gr. mould. I did find the exact same mould in a 240 something grain, same nose, just shorter at base.